Polycrystalline CVD Diamond

Comparing CDX, CDA and CDP

Hardness, modulus, thermal conductivity, breaking strength and wear resistance of our three mechanical grade CVD diamonds, side by side.

Comparing the performance parameters of CDX, CDA and CDP

PropertyCDXCDACDP
Vickers hardness (kg/mm²)8000100008000
Density (g/cm³)3.523.523.52
Young's modulus (GPa)85011001100
Thermal conductivity (W/cm·K)600 – 8001000 – 15001000 – 1200
Chemical stabilityDoes not dissolve in any acid or alkaliDoes not dissolve in any acid or alkaliDoes not dissolve in any acid or alkali
Breaking strength (MPa, 0.5 mm thickness)450600500
Thermal stability800 °C800 °C800 °C
Wear resistance ratio (× 10,000)10 – 2035 – 5520 – 30
CDXBlack, opaque hot-filament CVD diamond for applications where high wear resistance is required.View grade CDALight yellow-green, translucent DC arc plasma jet CVD diamond with the highest wear resistance in the range.View grade CDPCost-effective DC arc plasma jet CVD diamond with a wear resistance ratio below CDA.View grade